ELECTRODES FOR SURFACING, OVERLY & HARDFACING APPLICATION
High Resistance to Abrasion Moderate impact at elevated temperature
Basis OF Alloys : C, Cr, Mn, Ni
CHARACTERISTICS : Basic coated, Hard facing electrode for achieving high deposition efficiency 170% approx. High resistant to abrasion due to high content of chromium and carbon .machining by grinding. Resistant to heavy mineral abrasion and moderate.
APPLICATION :
RE-DRY CONDITION : Re-Dry the electrode at 250°C-300°C for 1 hour,
ALL WELD CHEMICAL COMPOSITION %:
C |
Mn |
Si |
Cr |
Ni |
5.0 max. |
1.00 max. |
2.00 max |
24-28 |
3.50-4.50 |
WELD METAL HARDNESS:
As welded Hardness |
56-62 HRC |
DIEMENSION, CURRENT CONDITION & PACKING DATA:
Size(mm) |
Size(inch) |
Current Condition |
weight of |
Weight of Case |
(Dia) |
(Dia) |
(DC+/ AC) Amps |
packet |
|
|
|
|
(Kgs) |
|
3.15/ 3.20 X 350 |
1/ 8” X 14” |
100-130 |
5 |
20 |
4.00 X 350 |
5/ 32” X 14” |
150-180 |
5 |
20 |
5.00 X 350 |
3/ 16” X 14” |
210-260 |
5 |
20 |