High resistance to abrasion with moderate impact at elevated temperature.
C, Cr
Basic coated hard facing electrode for achieving high deposition efficiency (~170%). Highly resistant to abrasion due to high chromium and carbon content. Can be machined by grinding. Resistant to heavy mineral abrasion and moderate impact.
Re-Dry the electrode at 250°C–300°C for 1 hour.